돌아가기
Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
HRID 1016220생성일: 2026년 10월 26일

Nitric Acid → Zinc Phosphate

https://huagongshe.com/reaction/1016220

반응식

참여 물질

역할이름HCID투입량
반응물Nitric AcidHCID 944—
반응물Phosphoric AcidHCID 1004—
반응물Zinc NitrateHCID 24518—
용매WaterHCID 962—
생성물Zinc PhosphateHCID 24519—

반응 단계

Phosphating solution based on zinc diacid phosphate, nitric acid, zinc nitrate and phosphoric acid in a percentage amount, diluted in water, of between 5 and 20%, at a temperature of 60-85° C. for a variable between 5 and 15 minutes, so as to produce a compact and homogeneous zinc phosphate coating with a very fine crystalline structure so as to facilitate mechanical deformation of the cold material;

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US06474127B1
출처 데이터셋uspto-grants-2002_11
ORD IDord-3378e7dc71c34c4db4750d839dffb11e
출처 메모uspto-grants-2002_11