반응식
[OH-].[Al+3:2].[OH-].[OH-].[C:5]([OH:10])(=[O:9])[CH:6]([CH3:8])[OH:7]>O>[C:5]([O-:10])(=[O:9])[CH:6]([CH3:8])[OH:7].[Al+3:2].[C:5]([O-:10])(=[O:9])[CH:6]([CH3:8])[OH:7].[C:5]([O-:10])(=[O:9])[CH:6]([CH3:8])[OH:7]참가 물질
4
반응 조건
- 온도
- 343 K
실험 절차
Aluminum(III) hydroxide (2.21 g) was suspended with stirring (340 rpm) in water (10.8 g) maintained at 343 K, lactic acid (6.97 g) added over 1 minute, and stirring continued at 343 K for 70 hours. A white suspension was obtained, and this was diluted to 6% w/w solids for testing.
후처리
- customA white suspension was obtained
- additionthis was diluted to 6% w/w solids for testing
출처 및 근거
- ORD 기록
- ord-1999d9fe28034792b4b9767334223317
- 출처 데이터셋
- uspto-grants-2013_10
- 특허 번호
- US08562736B2
연결된 노트