참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | 3,3-Dimethyl-1-butene | HCID 11210 | — |
| 반응물 | Methyl 9-decenoate | HCID 1778877 | — |
| 용매 | Toluene | HCID 1140 | — |
| 생성물 | Methyl Decenoate Neohexene | HCID 131735995 | — |
반응 단계
10 g of methyl 9-decenoate (54 mmol) purified on alumina, 18.1 g of 3,3-dimethyl-1-butene (neohexene, 215 mmol, 4 equivalents) and 100 g of toluene are placed in a 250 ml 10 glass reactor purged with nitrogen. The mixture is heated at 40° C., followed by addition, over a period of 2 hours, of 3.4 mg of catalyst M73-SiPr supplied by the company Umicore (75 ppm mol) dissolved in 5 ml of toluene. At the end of the addition, the degree of conversion of the methyl decenoate, measured by CPG, is 86%. The selectivity toward cross metathesis product is 35%.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US09382189B2 |
|---|
| 출처 데이터셋 | uspto-grants-2016_07 |
|---|
| ORD ID | ord-223caae88ada44d4946ee5d8fb84ba8a |
|---|
| 출처 메모 | uspto-grants-2016_07 |
|---|