돌아가기
Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
HRID 1076944생성일: 2026년 10월 26일

Azobisisobutyronitrile → Vinyl acetate sodium ethylenesulfonate

https://huagongshe.com/reaction/1076944

반응식

참여 물질

역할이름HCID투입량
반응물AzobisisobutyronitrileHCID 6547—
반응물Vinyl AcetateHCID 7904—
반응물Sodium vinylsulfonateHCID 3270262—
용매MethanolHCID 887—
생성물Vinyl acetate sodium ethylenesulfonateHCID 131710246—

반응 단계

A 1,000 ml. glass polymerization vessel equipped with a reflux condenser, a dropping funnel, a thermometer and a stirrer was charged with 320 parts of vinyl acetate, 130 parts of methanol, 15 parts of 30% aqueous solution of sodium ethylenesulfonate and 0.2% by mole of azobisisobutylonitrile per the vinyl acetate. After carrying out the polymerization at a temperature of 60° to 65°C. for 8 hours, the residual vinyl acetate was removed by a conventional method to give vinyl acetate-sodium ethylenesulfonate copolymer containing 2.3% by mole of sodium ethylenesulfonate unit. Then the copolymer was hydrolyzed by a conventional method to give a modified PVA of which degree of hydrolysis in vinyl acetate unit was 99% by mole.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US03959205
출처 데이터셋uspto-grants-1976_05
ORD IDord-3cd5ee600b35427fb7f893bffc505f65
출처 메모uspto-grants-1976_05