반응 단계
this polymer material was produced by adding to 320 g xylene at 100° C. the monomer solution and a catalyst solution over a period of 3 hours. The monomer solution contained 2.900 g ethyl acrylate, 76 g acrylonitrile, 76 g acrylic acid and 3 g laurylmercaptan. The catalyst solution contained 26 g laurylperoxide and 7 g butylperbenzoate in 273 g of xylene. The material was highly viscous with comonomer proportions of 95:2.5:2.5.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US04965117 |
| 출처 데이터셋 | uspto-grants-1990_10 |
| ORD ID | ord-3302c6cf61fb48c19c71da6e8611e7f0 |
| 출처 메모 | uspto-grants-1990_10 |