(+-)-Pantolactone → Keto-pantoyllactone
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | (+-)-Pantolactone | HCID 989 | — |
| 촉매 | Molybdenum trioxide | HCID 14802 | — |
| 촉매 | Hematite (Fe2O3) | HCID 14833 | — |
| 생성물 | Keto-pantoyllactone | HCID 39 | — |
반응 단계
A mixture of iron (III) oxide and molybdenum trioxide (G-105 from Girdler) is used as the catalyst in the reactor described in Example 1 and the temperature of the air bath is adjusted to 225° C. 60 l of air and 33 g of pantolactone are subsequently added hourly to the evaporator. 96% of the pantolactone are transformed and ketopantolactone is formed with a selectivity of 83%.