| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Di-n-butyldilauryltin | HCID 9809426 | — |
| 반응물 | Mercaptoisocyanate | HCID 22024120 | — |
| 생성물 | Azelaic Acid | HCID 2266 | — |
반응 단계
About 50 grams of the mercaptoisocyanate solution prepared in Example 1 along with 0.01 g of dibutyltin dilaurate should be added to about 40 grams of the above prepared polyester and heated for about 3 hours at 100° C. to form a polyester having reactive mercapto groups.