| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Adipic Acid | HCID 196 | — |
| 반응물 | Succinic anhydride | HCID 7922 | — |
| 반응물 | Neopentyl glycol | HCID 31344 | — |
| 반응물 | Butanediol | HCID 165788 | — |
| 생성물 | Epoxide resin | HCID 16213861 | — |
반응 단계
77 g (0.05 equivalent) of an acid polyester prepared, by the melt process, from 21 mols of succinic anhydride and 20 mols of butanediol and 35 g (0.05 equivalent) of an acid polyester prepared, by the melt process, from 8 mols of adipic acid and 7 mols of neopentylglycol are warmed to 120° C. and mixed well with 11.0 g (0.1 equivalent) of triglycidyl isocyanurate and the mixture is poured into Anticorodal moulds which have internal dimensions of 150×150×1 mm, have been treated with a silicone mould-release agent and have been pre-warmed to 140° C. After removing the air, the mixture is cured in vacuo for 16 hours at 140° C. Crystalline, soft and tough mouldings are obtained, on which the following characteristics are determined:
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US04259198 |
|---|
| 출처 데이터셋 | uspto-grants-1981_03 |
|---|
| ORD ID | ord-4077398a68c449bd94eb8bde13a2dfec |
|---|
| 출처 메모 | uspto-grants-1981_03 |
|---|