Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Toluene → 1-Ethenyl-4-methylbenzene
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Toluene | HCID 1140 | — |
| 반응물 | Methylalumoxane | HCID 23511181 | — |
| 촉매 | HCID 178420299 | HCID 178420299 | — |
| 생성물 | 1-Ethenyl-4-methylbenzene | HCID 12161 | — |
반응 단계
A syndiotactic poly-p-methyl-styrene in powder form is prepared according to the method described in Macromolecules, 1989, 22, 104. p-Methyl-styrene (0.5 mmoles) is polymerized in toluene (59 ml) at 50° C. for 24 hours, in the presence of tetrabenzyltitanium (5·10 moles) and methylalumoxane (0.3 g); 8.5 g of s-PpMS are obtained. A film about 100 microns thick is produced by compression molding at a pressure of 2 Kg/cm2 and at a temperature of 230° C. An amorphous film is thus obtained.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US05468823 |
| 출처 데이터셋 | uspto-grants-1995_11 |
| ORD ID | ord-0d799e0068c248149064b0a182c8fd07 |
| 출처 메모 | uspto-grants-1995_11 |