반응식
[C:1](OC)(=[O:12])[C:2]1[CH:11]=[CH:10][C:5]([C:6]([O:8]C)=[O:7])=[CH:4][CH:3]=1.[CH2:15]([OH:20])[CH2:16][CH2:17][CH2:18][OH:19].CCOP(SCSP(OCC)(OCC)=S)(OCC)=S>CC([O-])C.CC([O-])C.CC([O-])C.CC([O-])C.[Ti+4]>[CH2:10]1[O:8][CH2:6][CH2:5]1.[C:1]1(=[O:12])[O:20][CH2:15][CH2:16][CH2:17][CH2:18][O:19][C:6](=[O:7])[C:5]2[CH:10]=[CH:11][C:2]1=[CH:3][CH:4]=2참가 물질
5
실험 절차
Poly(trimethylene ether-tetramethylene terephthalate) was prepared as described for Example 1, with the exception that the number average molecular weight of the polytrimethylene ether glycol used was 2,390. The amounts of ingredients used were: dimethyl terephthalate, 12.52 kg; 1,4-butanediol, 14.90 kg; polytrimethylene ether glycol, 13.0 kg; tetraisopropyl titanate, 43.3 g; and ETHANOX, 80.8 g. The properties of the elastomer are reported in Table 1.
출처 및 근거
- ORD 기록
- ord-d7bbcb752039456cb237918c433753b3
- 출처 데이터셋
- uspto-grants-2007_07
- 특허 번호
- US07244790B2
연결된 노트