참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Formaldehyde | HCID 712 | — |
| 반응물 | Sulfur Dioxide | HCID 1119 | — |
| 반응물 | Urea | HCID 1176 | — |
| 반응물 | Melamine | HCID 7955 | — |
| 용매 | Water | HCID 962 | — |
| 용매 | O-Xylene | HCID 7237 | — |
| 생성물 | Urea, polymer with formaldehyde and 1,3,5-triazine-2,4,6-triamine | HCID 168250 | — |
반응 단계
A urea-formaldehyde-melamine prepolymer solution is prepared from 165 grams of 37% aqueous formaldehyde, 45 grams of water, 89 grams of urea and 1 gram of melamine, adjusted to pH 9.3 and heated for 1 hour at 65° C. 170 grams of this prepolymer solution are emulsified in a solution of 6 grams of Tetronic 1502 dissolved in 100 grams of xylene, and 0.06 milliequivalents of sulfur dioxide (about 4 normal in xylene solution) is added, resulting in an exothermic reaction. After stirring for 1 hour, the solvent dispersion has little or no precipitate. Without any preliminary phase separation, the product is mixed with water to give about 16% total solids, and this "aqueous redispersion" is steam distilled under high-shear agitation to yield a product free of residual xylene, closely resembling that described in Example 1. A paper coating prepared as described in Example 1 has a scatter coefficient of about 4,000 cm2 /gram.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US04058434 |
|---|
| 출처 데이터셋 | uspto-grants-1977_11 |
|---|
| ORD ID | ord-09fdc8cd40fb42a9b47e86718552c886 |
|---|
| 출처 메모 | uspto-grants-1977_11 |
|---|