Methyl Methacrylate → Methyl Methacrylate
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Methyl Methacrylate | HCID 6658 | — |
| 반응물 | Potassium Persulfate | HCID 24412 | — |
| 반응물 | Diethylaminoethyl Methacrylate | HCID 61012 | — |
| 반응물 | Ethylene glycol diacrylate | HCID 75282 | — |
| 반응물 | Emulphor | HCID 5364713 | — |
| 반응물 | Sodium Bisulfite | HCID 23665763 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | Methyl Methacrylate | HCID 6658 | — |
| 생성물 | 2-(Diethylamino)ethyl acrylate | HCID 17050 | — |
반응 단계
50 Grams of N,N-diethylaminoethyl methacrylate, 50 g. of methyl methacrylate, 1 g. of Dupanol ME, 1 g. of Emulphor ON-870, 6 g. of ethylene diacrylate, 1 g. of potassium persulfate, and 0.5 g. of sodium bisulfite are dissolved or mixed with 1,000 g. of water. This mixture is tumbled in a water bath at 60° C. for 24 hr. to obtain a crosslinked copolymer of methyl methacrylate and N,N-diethylaminoethyl acrylate. The crosslinked polymer is separated from the aqueous dispersion by the method described in Example 4.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US04177255 |
| 출처 데이터셋 | uspto-grants-1979_12 |
| ORD ID | ord-efb2909c87374da8ab769c9d65862d66 |