Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
3-Methyl-1-butene → 3-Methyl-1-butene 4-methyl-1-pentene
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | 3-Methyl-1-butene | HCID 11239 | — |
| 반응물 | 4-Methyl-1-pentene | HCID 12724 | — |
| 생성물 | 3-Methyl-1-butene 4-methyl-1-pentene | HCID 86745312 | — |
반응 단계
A random copolymer was prepared in the same manner as described in (2) above except that 1.65 kg of a mixture of 3-methyl-1-butene with 4-methyl-1-pentene at a weight ratio of 1/0.65 was supplied at a rate of 0.41 kg/hr instead of 1.0 kg of 3-methyl-1-butene supplied at a rate of 0.25 kg/hr. The crystallization degree of the polymer obtained was 54.0%.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US05075381 |
| 출처 데이터셋 | uspto-grants-1991_12 |
| ORD ID | ord-7098dda66cca4082be79ed5f870e8201 |
| 출처 메모 | uspto-grants-1991_12 |