반응물PhenolHCID 996—
반응물AluminumHCID 5359268—
생성물Phenol, aluminum salt (3:1)HCID 167236—

반응 조건

온도150 °C

반응 단계

In a reaction vessel was placed 8100 parts of phenol and 27 parts of aluminum metal. The vessel was sealed and heated to 150° C. to form aluminum triphenoxide. This catalyst concentrate was then mixed with 11,124 parts of additional phenol. This gives a phenol/aluminum mole ratio of about 203. The phenol-catalyst mixture was cooled to 90° C. and 23,490 parts of isobutylene was pumped in over a 50-minute period. The reaction temperature rose to 110° during the first 10 minutes of isobutylene feed. Stirring was continued at 110°-115° C. for 165 minutes. Reactor pressure dropped to 120 psig from a maximum of 260 psig.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US04870215
출처 데이터셋uspto-grants-1989_09
ORD IDord-8d821badf57d4ee381083a26d3e3255c
출처 메모uspto-grants-1989_09