참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Vinyl Acetate | HCID 7904 | — |
| 반응물 | Maleic Anhydride | HCID 7923 | — |
| 반응물 | Di-tert-butyl peroxide | HCID 8033 | — |
| 용매 | O-Xylene | HCID 7237 | — |
| 생성물 | Acetic acid ethenyl ester, polymer with 2,5-furandione | HCID 269112 | 87% |
반응 단계
73.5 parts by weight of maleic anhydride and 21.4 parts by weight of vinyl acetate were dissolved in 240 parts by volume of xylene and heated to 70° C. 4.5 parts by weight of ditertiary butyl peroxide in 20 parts by volume of xylene were added and the reaction mixture was heated to 130° C. and maintained at this temperature for 3 hours. A brown resin precipitated, which on cooling solidified, and was easily separated from the bulk of the xylene by decantation. Yield = 87% (on weight of monomers). The number average molecular weight of the polymer by vapour phase osmometry was found to be 675.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US04126549 |
|---|
| 출처 데이터셋 | uspto-grants-1978_11 |
|---|
| ORD ID | ord-a6b68616e44d4cad8bc9ed8bea921397 |
|---|
| 출처 메모 | uspto-grants-1978_11 |
|---|