Urea → Dipropylene glycol monocarbamate

https://huagongshe.com/reaction/1706297

반응식

참여 물질

역할이름HCID투입량
반응물UreaHCID 1176—
반응물2-(2-Hydroxypropoxy)-1-propanolHCID 32881—
반응물HO-Peg18-OHHCID 14497137—
촉매NickelHCID 935—
생성물Dipropylene glycol monocarbamateHCID 13171178576%

반응 조건

온도155 °C

반응 단계

810 parts of a polyethylene ether-diol of molecular weight 810 (H(OCH2CH2)18OH) and 60 parts of urea are heated in a stirred apparatus for 5 hours at 150° C., whilst passing a stream of nitrogen through the apparatus. After this time, the degree of conversion is 92%. Thereafter, 2,680 parts of dipropylene glycol, 1,200 parts of urea and 100 parts of the nickel-containing exchanger prepared as described in Example 1(a) are added. The reaction mixture is heated for 16 hours at 155° C., whilst passing a stream of nitrogen through the apparatus. After the mixture has cooled to about 100° C., the catalyst is filtered off. 4,350 parts of the co-carbamate mixture, consisting of 24% of a polyethylene ether-diol monocarbamate H(OCH2CH)18OCONH2 and 76% of dipropylene glycol monocarbamate, are obtained.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US04207073
출처 데이터셋uspto-grants-1980_06
ORD IDord-39a8d7ed0537482c91707f3d2552054e
출처 메모uspto-grants-1980_06