참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Benzoyl Peroxide | HCID 7187 | — |
| 반응물 | Glycidyl methacrylate | HCID 7837 | — |
| 반응물 | 2-Ethylhexyl methacrylate | HCID 12713 | — |
| 생성물 | 2-Ethylhexyl methacrylate-giycidyl methacrylate | HCID 86747971 | — |
반응 단계
To the above solvent, a mixture of 200 g of 2-ethylhexyl methacrylate, 10 g of glycidyl methacrylate and 2 g of benzoyl peroxide was added dropwise at a constant speed over a period of 2 hours, followed by stirring at 90° C. for 4 hours to complete the polymerization reaction. Thus, 2-ethylhexyl methacrylate - giycidyl methacrylate copolymer was obtained.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US05328794 |
|---|
| 출처 데이터셋 | uspto-grants-1994_07 |
|---|
| ORD ID | ord-d9b15d8727d74cf885b73d8610e98b6b |
|---|
| 출처 메모 | uspto-grants-1994_07 |
|---|