S(OOS([O-])(=O)=O)([O-])(=O)=O.[NH4+].[NH4+].[CH2:13]=[CH:14][C:15]1[CH:20]=[CH:19][CH:18]=[CH:17][CH:16]=1.[C:21]([OH:26])(=[O:25])[C:22]([CH3:24])=[CH2:23].[Na].S([O-])([O-])(=O)=O.C1OC1.C(O)(=O)C(C)=C>>[CH:13]([CH2:24][C:22](=[CH2:23])[C:21]([OH:26])=[O:25])=[CH:14][C:15]1[CH:20]=[CH:19][CH:18]=[CH:17][CH:16]=1참가 물질
6
실험 절차
Further, 30 parts of a 1% aqueous solution of ammonium persulfate were added thereto, and the mixture was aged for 5 hours at 75° C. Thus, an aqueous dispersion (i.e., a particulate resin dispersion (A2)) of a vinyl resin (i.e., a copolymer of styrene/methacrylic acid/sodium salt of sulfate of ethylene oxide adduct of methacrylic acid) was prepared.