1.8 g of the styrene-maleic anhydride polymer (molecular weight: 1600) was mixed with 5.4 g of the polyethyleneoxyglycol (molecular weight: 600). The mixture was dropped on a glass substrate and heated in an oven at 100° C. under nitrogen stream. After 30 hours, the mixture was cooled down to room temperature, immersed into methanol and dried. A thin membrane of the styrene-maleic acid polyethyleneoxy ester crosslinked copolymer of an excellent adhesive strength and mechanical strength was prepared.
후처리
- additionThe mixture was dropped on a glass substrate
- temperaturethe mixture was cooled down to room temperature
- customdried
출처 및 근거
- ORD 기록
- ord-68b8dcdabb4f48ecabf77603d936bffa
- 출처 데이터셋
- uspto-grants-2000_09
- 특허 번호
- US06123875
반응 노트
불러오는 중…