Phosphoric Acid → Yttrium oxide
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Phosphoric Acid | HCID 1004 | — |
| 반응물 | Yttrium | HCID 23993 | — |
| 반응물 | Yttrium oxide | HCID 159374 | — |
| 생성물 | Yttrium oxide | HCID 159374 | — |
| 생성물 | Yttrium phosphate | HCID 10313406 | — |
반응 단계
Generally, a 75 to 85 weight percent solution of phosphoric acid is added to the slurry over a period of about 15 minutes to about 90 minutes as the slurry is continuously agitated and maintained at a temperature that typically ranges between about 20° C. and about 70° C. The amount of the phosphoric acid added to the slurry is usually about 1.5 molar percent less than the amount of the yttrium compound present in the slurry. When the yttrium compound used is yttrium oxide, the reaction takes place to form yttrium phosphate, minor amounts of yttrium oxide, minor amounts of surface adsorbed phosphoric acid and water. The yttrium phosphate formed comprises approximately 95.5 percent of the solids portion in the slurry.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US08425871B2 |
| 출처 데이터셋 | uspto-grants-2013_04 |
| ORD ID | ord-6133381c1d1f40118090b7162bf7793b |
| 출처 메모 | uspto-grants-2013_04 |