참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | 4,4'-Dihydroxybiphenyl | HCID 7112 | — |
| 반응물 | Ethyltriphenylphosphonium acetate | HCID 94470 | — |
| 반응물 | 4,4'-Bis(2,3-epoxypropoxy)biphenyl | HCID 102824 | — |
| 반응물 | 2,7-Diglycidyloxy-1,3,4,5,6,8-hexamethyl-9-phenylxanthene | HCID 58746982 | — |
| 용매 | Methanol | HCID 887 | — |
| 용매 | Dimethylacetamide | HCID 31374 | — |
| 생성물 | Xanthene biphenylene | HCID 69049558 | 95% |
반응 단계
1.555 g (manufactured by DAINIPPON INK & CHEMICALS Co., Ltd., “EXA7335”, 3.2 mmol) of 2,7-diglycidyloxy-1,3,4,5,6,8-hexamethyl-9-phenylxanthene, 0.238 g (0.8 mmol) of 4,4′-diglycidyloxybiphenyl, 0.67 g (3.6 mmol) of 4,4′-dihydroxybiphenyl and 0.0106 g (0.02 mmol) of ethyltriphenylphosphonium acetate in a 70% methanol solution were reacted for 4 hours by stirring while heating to 160° C. in 2.463 g of N,N-dimethylacetamide under a nitrogen atmosphere. After cooling, a pale yellow transparent semi-solid reaction solution was diluted with 11.495 g of N,N-dimethylacetamide and then added dropwise in ice. The resulting white massive precipitate was suction-filtered, washed with ice water and then boiled in 200 ml of water for 30 minutes while vigorously stirring. After cooling, the precipitate obtained by decantation was ground and the powered precipitate was washed with water and methanol, and then vacuum dried at 60° C. to obtain a xanthene-biphenylene copolymer type linear epoxy resin. The amount of the resulting xanthene-biphenylene copolymer type linear epoxy resin was 2.33 g and the yield was 95%.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US07514507B2 |
|---|
| 출처 데이터셋 | uspto-grants-2009_04 |
|---|
| ORD ID | ord-d968195c09f1446da5e931a071bdfc9f |
|---|
| 출처 메모 | uspto-grants-2009_04 |
|---|