Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Sodium aluminate → Sodium aluminosilicate
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Sodium aluminate | HCID 14766 | — |
| 반응물 | Sodium orthosilicate | HCID 26051 | — |
| 생성물 | Sodium aluminosilicate | HCID 72941443 | — |
반응 단계
According to batch size, gel composition and contents of sodium silicate, sodium aluminate solution is prepared. This is added at a controlled rate and at ambient temperature to sodium silicate solution taken previously in a stainless steel reactor. Slurry of reaction mixture is allowed to crystallize at temperature 70-100° C. for 1 to 5 hours until Zeolite-A formation takes place. Zeolite-A slurry is filtered and washed till filtrate pH was ˜11 to 10.5. Wet cake thus obtained is dried in a dryer and dry powder was pulverized and subjected to analysis. The comparison of the properties of detergent builder Zeolite-A produced according to present invention (Example 10) and SASIL (Degussa-Henkel) is given in Table 1.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US07560093B2 |
| 출처 데이터셋 | uspto-grants-2009_07 |
| ORD ID | ord-a7b91d1aa1754fbbaf6a75c47af75f06 |
| 출처 메모 | uspto-grants-2009_07 |