Sodium Hydroxide → poly(vinyl alcohol-co-N-vinyl-2-pyrrolidone)
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Sodium Hydroxide | HCID 14798 | — |
| 반응물 | Ganex E 535 | HCID 270885 | — |
| 용매 | Methanol | HCID 887 | — |
| 생성물 | poly(vinyl alcohol-co-N-vinyl-2-pyrrolidone) | HCID 3082248 | 50.8% |
반응 단계
0.19 g (4.8 mmole) of sodium hydroxide was dissolved in 4.7 ml of methanol. The resultant solution was added to 800 mg of 1-vinylpyrrolidone/vinyl acetate copolymer (V). The mixture was stirred at room temperature for 48 hours. The hydrolyzed product, 1-vinyl pyrrolidone/vinyl alcohol copolymer was precipitated out in 10-fold excess of diethyl ether three times. The solid was then dried under vacuum at 60° C. overnight to yield 320 mg of 1-vinyl pyrrolidone/vinyl alcohol copolymer (VI). IR (KBr pellet): 3467.7, 2949.0, 1654.0, 1441.0, 1291.5, 649.9 cm-1: C-13 NMR, (D20) :17.6, 31.3, 33.6-35.1, 38.0-40.0, 42.6-45.9, 64.5-65.8.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US05686071 |
| 출처 데이터셋 | uspto-grants-1997_11 |
| ORD ID | ord-dd2803c335ee4abb8f52e70a6c31f341 |
| 출처 메모 | uspto-grants-1997_11 |