Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Tricalcium Phosphate → Hydroxylapatite (Ca5(OH)(PO4)3)
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Tricalcium Phosphate | HCID 24456 | — |
| 반응물 | Calcium Hydroxide | HCID 6093208 | — |
| 생성물 | Hydroxylapatite (Ca5(OH)(PO4)3) | HCID 14781 | — |
반응 단계
Basically, according to the present invention, an acidic calcium phosphate solution is reacted with a calcium hydroxide solution, with both solutions near saturation when combined, so as to obtain an amorphous hydroxylapatite precipitate without undesired side reactions. After separation and drying, hydroxylapatite precipitate is sintered at 700°-1100°C. for about 5-30 minutes to obtain the desired ceramic hydroxylapatite material.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US04849193 |
| 출처 데이터셋 | uspto-grants-1989_07 |
| ORD ID | ord-26014b10101f447c8a5611614776ac8f |
| 출처 메모 | uspto-grants-1989_07 |