반응식
O=C=[N:3]C1CC(C)(C)CC(C)(CN=C=O)C1.[C:17]([O:21][CH2:22][CH2:23]O)(=[O:20])[CH:18]=[CH2:19].C(O)(=O)C=C>>[C:17]([OH:21])(=[O:20])[CH:18]=[CH2:19].[NH2:3][C:17]([O:21][CH2:22][CH3:23])=[O:20]참가 물질
4
반응 조건
- 온도
- 70 °C
실험 절차
In a flask equipped with a stirrer, a thermometer and a reflux condenser, 222 parts of isophorone diisocyanate was charged. After heating to 70° C. while stirring, 116 parts of hydroxyethyl acrylate was added dropwise over one hour and reacted to obtain an intermediate. Then, in a flask equipped with a stirrer, a thermometer and a reflux condenser, 144 parts of acrylic acid was added to 376 parts of a bisphenol A epoxy resin (epoxy equivalent: 118 g/eq) and the reaction was conducted at 100° C. for 8 hours. To the reaction product, 338 parts of the above intermediate was added and the reaction was conducted at 80° C. for 5 hours to obtain a urethane acrylate (H-2) as a radical polymerizable oligomer (A1).
후처리
- customIn a flask equipped with a stirrer
- customreacted
- customto obtain an intermediate
- customThen, in a flask equipped with a stirrer
- additionTo the reaction product, 338 parts of the above intermediate was added
- waitthe reaction was conducted at 80° C. for 5 hours
출처 및 근거
- ORD 기록
- ord-d4140a65238a4f7c9408145b293d9837
- 출처 데이터셋
- uspto-grants-2005_02
- 특허 번호
- US06850682B2