Methylphosphonic acid → Aluminum methylphosphonate

https://huagongshe.com/reaction/234593

반응식

참여 물질

역할이름HCID투입량
반응물Methylphosphonic acidHCID 13818—
반응물Aluminum HydroxideHCID 10176082—
용매WaterHCID 962—
생성물Aluminum methylphosphonateHCID 2335494657.7%

반응 조건

온도160 °C

반응 단계

0.780 g of aluminum hydroxide, 1.47 g of methylphosphonic acid, and 6.64 g of water were mixed and stirred for 1 hour. Then the mixture was placed in an internal cylinder of Teflon in a stainless steel pressure-resistant vessel, which was placed in turn in a constant-temperature bath, and the mixture in the vessel was heated under autogenous pressure at 160° C. for 48 hours. After cooling to room temperature, suspended needle crystals were scooped out, washed with water, and dried in air, to obtain 0.97 g of aluminum methylphosphonate. The product gave essentially the same powder X-ray diffraction pattern as that in Example 4, and the product also contained a phase that gave essentially the same powder X-ray diffraction pattern as that in Example 1.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US05595952
출처 데이터셋uspto-grants-1997_01
ORD IDord-c1761b9049854099ae1e723c113b9ac4
출처 메모uspto-grants-1997_01