반응 단계
The procedure of Example II is repeated except that 20 grams of L-(-)-lactide, 30 grams of epsilon caprolactone and 0.0105 grams of pure stannous octoate are placed in a glass flask, blanketed with nitrogen, and heated for 45 hours at 140° to 142° C. The copolymer is tough and elastic and has good tensile strength and elongation properties. The copolymer has a GPC molecular weight of Mw =323,000 and Mn =180,000. DSC of the copolymer reveals a moderate amount of crystallinity with a melting point endo-therm of 42° C. and a glass transition temperature of -16° C. Physical properties of the polymer are shown in Table 1.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US04643734 |
| 출처 데이터셋 | uspto-grants-1987_02 |
| ORD ID | ord-769478c61fac4769bad876e5c34cdc48 |
| 출처 메모 | uspto-grants-1987_02 |