참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Ethylene carbonate | HCID 7303 | — |
| 촉매 | Sodium metaborate | HCID 145326 | — |
| 용매 | Diethylene Glycol | HCID 8117 | — |
| 생성물 | Carbon Dioxide | HCID 280 | 17.8% |
| 생성물 | Ethylene carbonate | HCID 7303 | 100% |
반응 단계
A 50:1 mole ratio of ethylene carbonate to diethylene glycol is heated with stirring under a nitrogen atmosphere for 45 hours at 160° C. using 1.0 percent sodium metaborate as catalyst to give 100 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 17.8 percent carbon dioxide. The catalyst is removed as in Example 1.