돌아가기
Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
HRID 258524생성일: 2026년 10월 26일

Acetaldehyde → Formaldehyde urea silicate

https://huagongshe.com/reaction/258524

반응식

참여 물질

역할이름HCID투입량
반응물AcetaldehydeHCID 177—
반응물Urea silicateHCID 86734903—
생성물Formaldehyde urea silicateHCID 86734902—

반응 단계

One mol by weight of metasilicic acid and one mol by weight of urea are mixed, heated to 95° to 150° C. for 20 to 60 minutes, until the reaction is substantially complete, thereby producing white granules of urea silicate. The said urea silicate is mixed into about one mol of acetoaldehyde in an aqueous solution and the urea silicate goes into solution. The unreacted metasilicic acid is filtered out. About 15% to 25% of said metasilicic acid is filtered out. The urea silicate formaldehyde solution is heated to 70° to 110° C. for 20 to 60 minutes, until the desired viscosity is obtained, thereby producing poly (formaldehyde urea silicate) resin. The resin may be produced as a thick clear resin or a solid, depending on the length of time the resin is heated.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US04033935
출처 데이터셋uspto-grants-1977_07
ORD IDord-9780204487e14043b91a7386f1fc2080
출처 메모uspto-grants-1977_07