C(=O)([O-])[O-:2].[Mg+2:5].[S:6](=[O:8])=[O:7]>>[S:6](=[O:2])([OH:8])[O-:7].[Mg+2:5].[S:6](=[O:2])([OH:8])[O-:7]참가 물질
3
실험 절차
According to the invention a method of recovering magnesia from magnesium carbonate containing raw material includes the steps of forming a slurry of uncalcined raw material, heating the slurry to a temperature between 40° and 90° C., treating the slurry with sulphur dioxide to form soluble magnesium bisulphite, separating undissolved impurities from the solution of magnesium bisulphite, precipitating magnesium sulphite from the solution, separating the precipitate from the mother liquor and recovering magnesia from the separated precipitate.
후처리
- customof forming a slurry of uncalcined raw material
- temperatureheating the slurry to a temperature between 40° and 90° C.
출처 및 근거
- ORD 기록
- ord-e2ec1990de354442a2347f9662ca4e4b
- 출처 데이터셋
- uspto-grants-1979_05
- 특허 번호
- US04154802