참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Hydrochloric Acid | HCID 313 | — |
| 반응물 | Titanium Tetrachloride | HCID 24193 | — |
| 반응물 | Diammonium hydrogen phosphate | HCID 24540 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | Phosphoric acid, titanium(4+) salt (4:3) | HCID 159761 | — |
반응 단계
Titanium phosphate was prepared by the following procedure. Hydrochloric acid (500 g) was added to 5 liters of water, and 500 g of titanium tetrachloride was added dropwise at room temperature. After allowing the mixture to stand for 3 hours, a 10% aqueous solution containing 356 g of diammonium hydrogen phosphate was gradually added dropwise to the mixture with thorough stirring. After the formation of a precipitate, the system was allowed to stand at 70° C. for 6 hours. The precipitate was separated by filtration, and washed with water by means of a centrifugal separator until there was no chlorine ion in the filtrate. It was dried at 120° C., and then calcined at 550° C. for 3 hours. The resulting powder had the composition 2TiO2.P2O5 and a surface area, measured by the BET method, of 72 m2 /g.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US04018706 |
|---|
| 출처 데이터셋 | uspto-grants-1977_04 |
|---|
| ORD ID | ord-e9461f8b54bc40f79e6ec8feba94d9ad |
|---|
| 출처 메모 | uspto-grants-1977_04 |
|---|