In this experiment, a styrene-butadiene polymer was synthesized utilizing the continuous polymerization procedure of this invention. A two-reactor system which consisted of a 1-gallon first reactor and a 2-gallon second reactor was utilized with the polymerization temperature being maintained at about 190° F. (88° C.). In the procedure used, 1,3-butadiene was charged into the first reactor at a rate of 115.2 grams per minute, n-butyl lithium was charged into the first reactor as a 0.25M solution at a rate of 1.6 grams per minute and TMEDA was charged into the first reactor as a 0.25M solution at a rate of 1.04 grams per minute. The 1,3-butadiene monomer was charged into the reactor as a 16 weight percent premix solution in hexane. The residence time in the first reactor was 0.51 hours.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US05837756 |
|---|
| 출처 데이터셋 | uspto-grants-1998_11 |
|---|
| ORD ID | ord-acd1219300c04fc0871c4dfebf428277 |
|---|
| 출처 메모 | uspto-grants-1998_11 |
|---|