온도
85 °C

실험 절차

Then, 58 g of styrenated phenol, 44 g of dilaurylthiodipropionate, and 58 g of triphenyl phosphite were added to the obtained polymer latex. The mixture was coagulated at 50° C. with an aqueous 0.25% sulfuric acid so that the latex/water ratio was 1/2, and the mixture was maintained at 85° C. for 5 minutes.