Formaldehyde → Crl-8131

https://huagongshe.com/reaction/371780

반응식

참여 물질

역할이름HCID투입량
반응물FormaldehydeHCID 712—
반응물Sulfuric AcidHCID 1118—
반응물UreaHCID 1176—
반응물TriethanolamineHCID 7618—
반응물Crl-8131HCID 24751—
반응물Sorbitan mono-(9Z)-9-octadecenoateHCID 9920342—
반응물Span #80 (Sorbitan monooleate)HCID 70693544—
반응물HCID 178435162HCID 178435162—
촉매Titanium oxide (Ti3O)HCID 162651—
용매WaterHCID 962—
용매O-XyleneHCID 7237—
생성물Crl-8131HCID 24751—
생성물Urea formaldehyde foamHCID 62705—

반응 단계

A urea-formaldehyde prepolymer solution is prepared by heating an aqueous solution of two-hundred-twenty grams of 37% formaldehyde and 82 grams of urea, adjusted to pH 8 with triethanolamine, at 70° C for one hour. Fifty grams of this prepolymer solution are mixed with thirty grams of a 50% by weight dispersion of titanium dioxide in distilled water, and adjusted to pH 6 with dilute sulfuric acid. The aqueous dispersion is emulsified in a solution of six grams of Pluronic L122, three grams of sorbitan monooleate (commerically available as Span 80 from ICI America) and 1.5 grams of a poly(oxyethylene)-poly(oxypropylene) block copolymer with 30% poly(oxyethylene) and a molecular weight of about 2500 (commercially available as Pluronic L 63) in one-hundred grams of xylene to yield a water-in-oil emulsion. This is treated with four milliliters of a 50% by weight solution of monobutyl acid phosphate in toluene and stirred for two hours.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US04087581
출처 데이터셋uspto-grants-1978_05
ORD IDord-b9e5ab78aa404bacaa0993020cdab82a
출처 메모uspto-grants-1978_05