참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Styrene | HCID 7501 | — |
| 반응물 | 1,3-Butadiene | HCID 7845 | — |
| 반응물 | Cyclohexane | HCID 8078 | — |
| 반응물 | Butyllithium | HCID 178418339 | — |
| 용매 | Tetrahydrofuran | HCID 8028 | — |
| 생성물 | Styrene-butadiene-styrene | HCID 22280236 | — |
반응 단계
In a 2 gallon autoclave reactor, 4,500 g of cyclohexane was placed. 9 g of tetrahydrofuran, 112.5 g of styrene monomer and 1.3 g of n-butyllithium were charged into the reactor and then the reaction mixture was subjected to polymerization for 1 hour. Thereafter, 525 g of 1,3-butadiene monomer was injected into the reactor to polymerize for one hour. Finally, 112.5 g of styrene monomer was added and then polymerized for one hour to obtain styrene-butadien-styrene living block copolymer with a number average molecular weight of about 100,000 which had a styrene content of 29.9% (block styrene content of 29.5%) and 1,2-vinyl bond content of 39.6% (27.9% when reduced into whole polymer). Living lithium in the polymer was present in an amount of 1.00 mmol per 100 g of polymer.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US06020439 |
|---|
| 출처 데이터셋 | uspto-grants-2000_02 |
|---|
| ORD ID | ord-f7736a74c74a44e19187a776e49ec4d0 |
|---|
| 출처 메모 | uspto-grants-2000_02 |
|---|