Ammonia → Nickel cobalt magnesium hydroxide
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Ammonia | HCID 222 | — |
| 반응물 | Sodium Hydroxide | HCID 14798 | — |
| 반응물 | Cobalt dinitrate | HCID 25000 | — |
| 반응물 | Magnesium nitrate | HCID 25212 | — |
| 반응물 | Nickel nitrate | HCID 25736 | — |
| 생성물 | Nickel cobalt magnesium hydroxide | HCID 71350743 | — |
반응 단계
In this way, the reaction was conducted for 48 hours while continuously adding the aqueous solution of mixture of nickel nitrate, cobalt nitrate and magnesium nitrate, the aqueous ammonia and the aqueous solution of sodium hydroxide to the reactor. During the reaction, the concentration of ammonia in the reaction mixture (slurry) in the reactor was kept within a range from 1.0 to 1.3 mol/L and the reaction temperature was kept at 30° C.±1° C. with a temperature controller. After the completion of the reaction, the slurry in the reactor was filtered, lashed with water and dried to provide a powder of nickel cobalt magnesium hydroxide.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US06306787B1 |
| 출처 데이터셋 | uspto-grants-2001_10 |
| ORD ID | ord-6cfd1fdac17d4895b989fa0039bea66b |
| 출처 메모 | uspto-grants-2001_10 |