Ammonia → Nickel cobalt aluminum hydroxide
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Ammonia | HCID 222 | — |
| 반응물 | Sodium Hydroxide | HCID 14798 | — |
| 반응물 | Cobalt dinitrate | HCID 25000 | — |
| 반응물 | Nickel nitrate | HCID 25736 | — |
| 반응물 | Aluminum nitrate | HCID 26053 | — |
| 생성물 | Nickel cobalt aluminum hydroxide | HCID 86204838 | — |
반응 단계
In this way, the reaction was conducted for 48 hours while continuously adding the aqueous solution of mixture of nickel nitrate, cobalt nitrate and aluminum nitrate, aqueous ammonia and the aqueous solution of sodium hydroxide to the reactor and continuously taking the resulting reaction mixture (slurry) out of the reactor. After 48 hours from the start of the reaction, the resulting slurry was filtered, washed with water and dried to provide a powder of nickel cobalt aluminum hydroxide.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US06306787B1 |
| 출처 데이터셋 | uspto-grants-2001_10 |
| ORD ID | ord-6ed6dd1301174c97ad055a0c7e8df58f |
| 출처 메모 | uspto-grants-2001_10 |