돌아가기
Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
HRID 384583생성일: 2026년 10월 25일

Styrene → Butyl prop-2-enoate;styrene

https://huagongshe.com/reaction/384583

반응식

참여 물질

역할이름HCID투입량
반응물StyreneHCID 7501—
반응물Butyl AcrylateHCID 8846—
반응물Potassium PersulfateHCID 24412—
반응물PotassiumHCID 5462222—
용매WaterHCID 962—
생성물Butyl prop-2-enoate;styreneHCID 168422—

반응 조건

온도60 °C

반응 단계

In a 200-liter reactor equipped with a stirrer, a cooling apparatus, a condenser and a monomer supplying tube, 5 parts by weight of butylacrylate, 15 parts by weight of styrene, 0.2 parts by weight of triallyl isocyanurate, 140 parts by weight of ion-exchanged water and 1.0 parts by weight of potassium rosinate are added and mixed. The temperature is raised to 60° C. with stirring. After 10 minutes from the time of reaching 60° C., 0.25 parts by weight of potassium persulfate dissolved in deionized water is added thereto to initiate polymerization. The temperature of the reactor is maintained at 70° C. for 60 minutes. The polymerization is carried out at 70° C. for an additional 30 minutes to give an inner core of butylacrylate-styrene copolymer.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US08367770B2
출처 데이터셋uspto-grants-2013_02
ORD IDord-6308c29c53df4acabed5aeb9c47e1454
출처 메모uspto-grants-2013_02