Phosphoric Acid → Zirconium phosphate

https://huagongshe.com/reaction/400319

반응식

참여 물질

역할이름HCID투입량
반응물Phosphoric AcidHCID 1004—
반응물ZirconiumHCID 23995—
반응물Zirconium hydroxide (Zr(OH)4), (T-4)-HCID 84465—
반응물PhosphorusHCID 5462309—
용매WaterHCID 962—
생성물Zirconium phosphateHCID 160986—

반응 조건

온도80 °C

반응 단계

Catalyst preparation. A zirconium phosphate based catalyst was prepared by a co-precipitation method. A solution of zirconium hydroxide (Zr(OH)4) as a zirconium precursor was dissolved in deionized water. To this solution, a stoichiometric amount of phosphoric acid as a phosphorus precursor was added. The resulting mixture was heated at 80° C. for 2 hours to remove water, and a paste was obtained. The resulting paste was then dried in an oven at 100° C. overnight (about 12-18 hours) to remove the bulk of any remaining water, and to provide a powder. The powder was then calcined at 350° C. for 2 hours to obtain powdered zirconium phosphate.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US08741258B2
출처 데이터셋uspto-grants-2014_06
ORD IDord-5158bc0245e144c6ba10bfddbe185877
출처 메모uspto-grants-2014_06