참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Azobisisobutyronitrile | HCID 6547 | — |
| 반응물 | 2-(Dimethylamino)ethyl acrylate | HCID 17111 | — |
| 반응물 | 11-(Methacryloylamino)undecanoic acid | HCID 2764185 | — |
| 용매 | Methanol | HCID 887 | — |
| 생성물 | MAU 2-(N,N-dimethylamino)ethyl acrylate | HCID 131731616 | 162.4% |
반응 단계
In 59.68 g of methanol were dissolved 18.88 g (70.12 mmol) of 11-methacrylamidoundecanoic acid (MAU), 1.12 g (7.79 mmol) of 2-(N,N-dimethylamino)ethyl acrylate (Tokyo Chemical industry Co.), and 0.32 g (1.95 mmol) of azobisisobutyronitrile (Nacalai Tesque, Inc.). The solution was deaerated by bubbling nitrogen for 60 minutes. The container was covered with a septum, and the polymerization was conducted by heating at 60° C. for 20 hours. After the completion of the polymerization reaction, the solution was concentrated to dryness under reduced pressure, and the solid was dissolved in 60 g of dimethylformamide. The obtained solution was dropwise added into a large excess of diethyl ether, and the resulting precipitate was collected by filtration under suction. After drying under reduced pressure, 5.22 g of random MAU/2-(N,N-dimethylamino)ethyl acrylate copolymer (90/10) was obtained (yield: 26.1%). The weight average molecular weight was 130000.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US08753686B2 |
|---|
| 출처 데이터셋 | uspto-grants-2014_06 |
|---|
| ORD ID | ord-37264b3a59d0413da954ad40b551bd50 |
|---|
| 출처 메모 | uspto-grants-2014_06 |
|---|