반응 단계
(A-2) 159 g of 3,3-bis (4-hydroxyphenyl)-2-benzofuran-1-on, 426.6 g of epichlorohydrin, and 160 g of a 50% alkali aqueous solution are mixed in a 1 L flask and reacted together at 95° C. for 1 hour to form a bisphenylbenzofuran-type epoxy resin. 215 g of the bisphenylbenzofuran-type epoxy resin is mixed with 450 mg of triethylbenzylammoniumchloride, 100 mg of 2,6-diisobutylphenol, and 72 g of acrylic acid. The mixture is heated up to 90 to 120° C. and completely dissolved, while air is blown therein at a speed of 25 Ml. Then, the dissolved product is cooled down to room temperature to form a non-colored transparent solid bisphenylbenzofuran-type epoxy acrylate. 287 g of the synthesized bisphenylbenzofuran-type epoxy acrylate is dissolved in 2 kg of cellosolveacetate. The solution is mixed with 10 g of 1,2,3,6-tetrahydrophthacid anhydride, 108.5 g of benzophenonetetracarboxylic acid dianhydride, and 1 g of tetraethylammonium bromide. The mixture is slowly heated up to 110 to 115° C. for 2 hours to form a cardo-based binder resin with a weight average molecular weight of 30,000 g/mol.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US08530537B2 |
|---|
| 출처 데이터셋 | uspto-grants-2013_09 |
|---|
| ORD ID | ord-c3add462b57c4a78aee913c31e254541 |
|---|
| 출처 메모 | uspto-grants-2013_09 |
|---|