참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Styrene | HCID 7501 | — |
| 반응물 | 1,3-Butadiene | HCID 7845 | — |
| 반응물 | N,N,N',N'-Tetramethylethylenediamine | HCID 8037 | — |
| 반응물 | 2,2'-Methylenebis(4-methyl-6-tert-butylphenol) | HCID 8398 | — |
| 반응물 | Butyllithium | HCID 178418339 | — |
| 용매 | Methanol | HCID 887 | — |
| 용매 | Toluene | HCID 1140 | — |
| 용매 | Cyclohexane | HCID 8078 | — |
| 생성물 | Styrene-butadiene-styrene | HCID 22280236 | — |
반응 단계
186 g of butadiene and 2.4 ml of a 0.5 M solution of tetramethylethylenediamine in cyclohexane is introduced into 4 litres of deaerated cyclohexane. After compensation for the impurities supplied by the solvent and the monomer using n-butyllithium, 3.7 ml of a 0.5 mol/l solution of n-butyllithium in cyclohexane is introduced. The polymerization of the polybutadiene block is effected at 60° C. After conversion of all the butadiene, 114 g of styrene is introduced, which is polymerized at 60° C. for 60 minutes. The copolymer is then protonated by addition of a large excess of methanol in solution in toluene, antioxidized by the addition of 2,2′- methylene bis(4-methyl-6-tert. butylphenol) (1 g per 100 g of monomer), then recovered by steam stripping and dried in an oven at reduced pressure at 60° C.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US06562923B1 |
|---|
| 출처 데이터셋 | uspto-grants-2003_05 |
|---|
| ORD ID | ord-247349b812b04a4781e5343d11f8e06f |
|---|
| 출처 메모 | uspto-grants-2003_05 |
|---|