Glycolide → HCID 178465153, 화합물

https://huagongshe.com/ko/reaction/412991

반응식

참여 물질

역할이름HCID투입량
반응물GlycolideHCID 65432—
반응물HCID 178435178HCID 178435178—
반응물HCID 178476396HCID 178476396—
용매WaterHCID 962—
용매N-methyl-2-pyrrolidoneHCID 13387—
생성물HCID 178465153HCID 178465153—

반응 단계

Poly(DL-lactide-co-glycolide) with a molar ratio of lactide to glycolide of 75/25 (Birmingham Polymer, Inc.) was dissolved in NMP to give a solution with 45% by weight polymer. This solution was filled into 3.0 cc polyproylene syringes with a male luer lock fitting and terminally sterilized by exposure to gamma irradiation at 23.2-24.6 kilograys. The polymer molecular weight after irradiation was 15,094 daltons. Leuprolide acetate was dissolved in water, sterile filtered through 0.2 mm filter and filled into a polypropylene syringe with a male luer lock fitting. The aqueous solution was frozen and the water removed by vacuum to yield a lyophilized cake of leuprolide. The two syringes were connected together with a coupler immediately prior to use and the contents of the two syringes mixed by moving the material back and forth between the two syringes for 40 cycles to provide a formulation with 6% by weight of leuprolide acetate. The product was then pulled into the syringe with the male luer lock fitting one a one-half inch 20 gauge needle attached.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US06565874B1
출처 데이터셋uspto-grants-2003_05
ORD IDord-99951c4a067a46c7b16d996c7f586156