반응식
[S:1].[CH2:2]1[CH:6]2[C@@H:7]3[CH:11]=[CH:10][C@H:9]([CH:5]2[CH:4]=[CH:3]1)[CH2:8]3.C(=O)([O-])[O-].[Ca+2]>O>[S:1].[CH2:2]1[CH:6]2[C@@H:7]3[CH:11]=[CH:10][C@H:9]([CH:5]2[CH:4]=[CH:3]1)[CH2:8]3참가 물질
5
반응 조건
- 온도
- 150 °C
실험 절차
Into a 4 liter autoclave were placed 425 g of sulfur, 75 g of DCPD, 2500 ml of water and 20 g of calcium carbonate. The reactor was then sealed and heated to 150° C. for three hours with stirring. After cooling to ambient temperature, the sulfur/DCPD adduct was isolated as small beads.
후처리
- customThe reactor was then sealed
- temperatureAfter cooling to ambient temperature
출처 및 근거
- ORD 기록
- ord-0005c5c1607a4f3f973b1472511c893f
- 출처 데이터셋
- uspto-grants-1988_12
- 특허 번호
- US04792589