Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Lauric Acid → Silver laurate
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Lauric Acid | HCID 3893 | — |
| 반응물 | Sodium Hydroxide | HCID 14798 | — |
| 반응물 | Silver Nitrate | HCID 24470 | — |
| 용매 | Water | HCID 962 | — |
| 용매 | Toluene | HCID 1140 | — |
| 생성물 | Silver laurate | HCID 9904644 | — |
반응 단계
1.9 g of sodium hydroxide was dissolved in 200 ml of water. To this solution, a solution of 12 g of lauric acid in 100 ml of toluene was added and the mixture was emulsified by stirring by with a stirrer. To this emulsion, an aqueous solution of silver nitrate (silver nitrate: 8.5 g, wafer: 50 cc) was added over a 60 second period while stirring the emulsion (800 r.p.m.; 5 minutes) to produce silver laurate. The precipitated silver laurate was removed and mixed with 30 g of polyvinyl butyral and 200 ml of isopropyl alcohol. The mixture was dispersed using of a ball mill to produce a polymer dispersion of the silver salt.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US04028129 |
| 출처 데이터셋 | uspto-grants-1977_06 |
| ORD ID | ord-0d727525b67c470daf48ad81e67cd1c2 |
| 출처 메모 | uspto-grants-1977_06 |