Sodium aluminate → Molecular sieve

HRID 442572

반응식

HRID 442572 반응식
O=[Al-:2]=O.[Na+:4].[Si:5]([O-])([O-:8])([O-:7])[O-:6].[Na+].[Na+].[Na+].[Na+]>>[O-:7][Si:5]([O-:8])=[O:6].[O-:7][Si:5]([O-:8])=[O:6].[Na+:4].[Al+3:2]

참가 물질

3

반응 조건

온도
75 °C

실험 절차

By using the same starting material as that of Example 1, the sodium aluminate solution was heated at 90° C. and stirred, and to which was mixed sodium silicate solution heated at 75° C. over a period of 12 minutes (maintaining a temperature of not lower than 80° C.) such that the total amount of the reaction solution was 5 kg in a 10-liter stainless steel container, in order to form a sodium aluminosilicate which as a whole was in a homogeneous gel-like form having the below-mentioned molar composition:

후처리

  1. temperaturemaintaining a temperature of not lower than 80° C.) such that the total amount of the reaction solution

출처 및 근거

ORD 기록
ord-834b15057c894397b5bc15a1d7785fcf
출처 데이터셋
uspto-grants-1999_04
특허 번호
US05891235

연결된 노트

불러오는 중…