Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Sulfuric Acid → Acrylonitrile butadiene styrene
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Sulfuric Acid | HCID 1118 | — |
| 반응물 | Styrene | HCID 7501 | — |
| 반응물 | 1,3-Butadiene | HCID 7845 | — |
| 반응물 | Acrylonitrile | HCID 7855 | — |
| 반응물 | Tetrasodium Pyrophosphate | HCID 24403 | — |
| 반응물 | (2R,3S,4R,5R)-2,3,4,5,6-pentahydroxyhexanal | HCID 107526 | — |
| 반응물 | Potassium Oleate | HCID 23665571 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | Acrylonitrile butadiene styrene | HCID 24756 | — |
반응 단계
50 parts of butadiene rubber latex powder, 36 parts of styrene, 14 parts of acrylonitrile, and 150 parts of deionized water were blended. To the blend, 1.0 parts of potassium oleate, 0.4 parts of cumenhydroperoxide, 0.2 parts of mercaptan-containing chain transfer agent, 0.4 parts of glucose, 0.01 parts of ferrous sulfate hydrate, and 0.3 parts of sodium pyrophosphate were added. The blend was kept at 75° C. for 5 hours to obtain g-ABS latex. To the g-ABS latex, 0.4 parts of sulfuric acid was added, coagulated and dried to obtain acrylonitrile-butadiene-styrene graft copolymer resin (g-ABS) in a powder form.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US07196126B2 |
| 출처 데이터셋 | uspto-grants-2007_03 |
| ORD ID | ord-6fffa5eb327f4108a8cf3204e8854c1c |
| 출처 메모 | uspto-grants-2007_03 |