Acrylamide → Acrylamide-acrylic acid resin

https://huagongshe.com/reaction/462480

반응식

참여 물질

역할이름HCID투입량
반응물AcrylamideHCID 6579—
반응물Acrylic AcidHCID 6581—
용매WaterHCID 962—
생성물Acrylamide-acrylic acid resinHCID 62693—

반응 조건

온도30 °C

반응 단계

56 grams 50% acrylamide, 12 grams acrylic acid and 127 grams water were mixed, and warmed up to 30° C. Nitrogen was used to purge the flask. Then 0.7 gram ammonium persulfate in 3 grams of water and 0.7 gram sodium metabisulfite in 3 grams water were added, respectively. After 20 minutes, the reaction began to take place, the temperature slowly rose to 78° C. (max.) after stirring for 1.5 hour a 20% copolymer was thus produced with an acrylamide/acrylic acid ratio of 70/30. 7 grams NaOH in 30 grams water was then added to neutralize the copolymer.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US04515855
출처 데이터셋uspto-grants-1985_05
ORD IDord-afb2cfbf8f8b4735958f3371f9372578
출처 메모uspto-grants-1985_05