Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Styrene → Acrylonitrile butadiene styrene
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Styrene | HCID 7501 | — |
| 반응물 | Acrylonitrile | HCID 7855 | — |
| 생성물 | Acrylonitrile butadiene styrene | HCID 24756 | — |
반응 단계
The procedure of Example i was repeated except a total of 273 grams of acrylonitrile was used instead of the total of 546 grams as per Example 1. In this example, the incremental addition was repeated except only one half of each amount of acrylonitrile was used. A portion of the latex was isolated for subsequent blending and the remaining latex coagulated as per Example 1. The dry rubber had a Mooney viscosity (100° C.) of 127, a bound acrylonitrile content of 3.8 weight percent (by Carlo Erba nitrogen analysis), a bound styrene content of 40.4 weight percent (by FTIR analysis) and a glass transition temperature of -28° C. (by DSC, Differential Scanning Calorimetry).
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US05225479 |
| 출처 데이터셋 | uspto-grants-1993_07 |
| ORD ID | ord-5bb327bb0c724325a400c352678e7fb0 |
| 출처 메모 | uspto-grants-1993_07 |