Aluminum nitrate nonahydrate → Dialuminium cobalt tetraoxide

HRID 483763
노트
인쇄 미리보기

반응식

HRID 483763 반응식
O.O.O.O.O.O.[N+]([O-])([O-])=[O:8].[Co+2:11].[N+]([O-])([O-])=[O:13].O.O.O.O.O.O.O.O.O.[N+]([O-])([O-])=[O:26].[Al+3:29].[N+]([O-])([O-])=[O:31].[N+]([O-])([O-])=[O:35].C(=O)([O-])[O-].[NH4+].[NH4+]>O>[O-2:8].[O-2:13].[O-2:26].[O-2:31].[O-2:35].[Al+3:29].[Al+3:29].[Co+2:11].[Co+2:11]
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

5

반응물 3

HCID 24567Aluminum nitrate nonahydrateHCID 24821Cobaltous nitrate hexahydrateHCID 517111Ammonium Carbonate

생성물 1

HCID 159384Dialuminium cobalt tetraoxide

시약·촉매·용매 1

HCID 962Water용매2회

실험 절차

In 300 ml of pure water were dissolved 29 g of cobalt nitrate hexahydrate and 75 g of aluminum nitrate nonahydrate. A solution of 38.4 g of ammonium carbonate dissolved in 100 ml of pure water was gradually added thereto with stirring to form a gel-form precipitate. The precipitate was washed with pure water three times, dried at 100° C. overnight and calcined at 600° C. in an air stream. The calcined material was then calcined at 800° C. in a muffle furnace for 3 hours to a cobalt aluminate catalyst having a blue color.

후처리

  1. additionwas gradually added
  2. customto form a gel-form precipitate
  3. washThe precipitate was washed with pure water three times
  4. customdried at 100° C. overnight
  5. customcalcined at 600° C. in an air stream

출처 및 근거